Article · Case Studies in Chemical and Environmental Engineering · July 16, 2024
Separation of iron and titanium from titanium magnetite raw materials by low-temperature treatment and magnetic separation
Galymzhan Maldybayev, Argyn Korabayev, R. A. Shayakhmetova, А.Т. Khabiyev, Omirserik Baigenzhenov, Rustam Sharipov
Abstract
This paper reviews a study on processing titanomagnetites using low-temperature treatment and magnetic separation. Using a reduction agent (15 %), chloride additives (15 %), and calcium fluoride (5 %) in low-temperature treatment reduced titanium magnetite iron content. This process extracted iron from titanium precisely and thoroughly. The best low-temperature treatment time and temperature were 60 minutes and 1200 °C. Magnetic separation with 0.2 T magnetic field intensity yielded 75.5 % magnetic fraction. Titanomagnetites treated at low temperatures had 50.9 % magnetic portion iron. Magnetic fraction iron extraction was 97.8 %. The yield of 24.5 % was achieved while the non-magnetic concentrate's titanium dioxide content grew to 65 %.
More by Omirserik Baigenzhenov
- Magnetic bentonite–keratin and bentonite–wool bio-composites as sorbents for magnetic dispersive micro-solid phase extraction of Pb(II) and Cd(II): Optimization and mechanistic insightsTalanta Open · 2026
- Adsorptive approaches for silicon recovery from industrial wastewater: materials, mechanisms, and recent advancesEgyptian Journal of Petroleum · 2026
- Valorization of Chrysotile Asbestos Waste into Hierarchically Porous Adsorbents for Thermal-Contact Demetallization of Heavy Oil: Mechanistic Insights and Process OptimizationInternational Journal of Technology · 2026
- Selective Nickel Recovery from the Magnetic Fraction of Chrysotile Asbestos Beneficiation Waste Using Organic AcidsInternational Journal of Technology · 2026